ok, I need someone to unconfuse me.
I went to a power coating place here in Austin to look around and get some pieces done (not for the T2, but I wanted to see how good of a job they would do).
Most of their work looked like the front of the BHSE, more like clear coat, which they said was a single step application process.
My question is, what do I have to ask for to get the finish that's on the rest of the BHSE, and something that makes sense for application to a heat sink? I forgot to ask, and next time I go back I'll bring a piece with me, but I just wanted to make sure I was a bit more informed.
In general, how think are the power coat layers, around 1 mil?
They didn't seem to know anything about polishing. They said that they scratch up the surface to help with adhesion anyways...