Licron is not available here and shipping anything under pressure is a no-go.  

The Comfort was available at my local store so I'll give it a go.  Nice consistency too and dirt cheap.  

Posted
17 minutes ago, spritzer said:

Licron is not available here and shipping anything under pressure is a no-go.  

The Comfort was available at my local store so I'll give it a go.  Nice consistency too and dirt cheap.  

Share a pic please, once you verify it works. BTW I bought Licron from Farnell, they had no trouble shipping it to an EU country.

Posted (edited)
5 hours ago, spritzer said:

Interesting, I'll see if I can find that locally.  Do you apply it with an airbrush or a sponge?  

Aumkar suggested to apply it with an airbrush, but I simply put a little on microfiber cloth and wipe it on the diaphragm.  After it dries, I buff it off.  It’s dirt cheap and working very well.  
 

Edited by chinsettawong
  • Like 2
  • Thanks 2
Posted
2 hours ago, ludoo said:

Share a pic please, once you verify it works. BTW I bought Licron from Farnell, they had no trouble shipping it to an EU country.

We aren't in the EU and that muddles everything.  

1 hour ago, chinsettawong said:

Aumkar suggested to apply it with an airbrush, but I simply put a little on microfiber cloth and wipe it on the diaphragm.  After it dries, I buff it off.  It’s dirt cheap and working very well.  
 

I'll try that plus I should have some airbrush equipment somewhere.  I just made some new stators for my Senn HD6x0 design that I want to try out.  

  • Like 1
Posted
7 hours ago, chinsettawong said:

Aumkar suggested to apply it with an airbrush, but I simply put a little on microfiber cloth and wipe it on the diaphragm.  After it dries, I buff it off.  It’s dirt cheap and working very well.  
 

But what about humidity? It doesn't seems to be immune for it.

Posted

Try an ATO alcohol solution with a concentration below 10% and add 1-2% volume of AEO7. This is the conductive coating I use now. It can make a transparent coating with a stable surface resistance of 10^8Ω

  • Thanks 1
Posted (edited)

My weakness I do not know these code words: ATO, AE07. I learned chemistry in a few decades ago if not in English.

....

I googled some Fatty Alcohol Polyoxyethylene Ether  and antimony doped tin-oxid. Where can you get these for kitchen tuning?

Edited by judo
  • Thanks 1
Posted (edited)

This can be a bit more complicated for example HCl is toxic in a short term NaCl is maybe in a long term :) Antimony is in some solders and it can react in the real world so it depends.

Afaik AOT is not toxic. I think you can not solve directly the powder in alcohol you have to make a colloide with very little particles. So I thought that solution may be available. I am only curious I do not need this in the minute and I do not want your "secrets" :) I asked about kitchen tuning because @Kung's highly pro achievements what I admire are definitely not available for me.

 

Edited by judo

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.